Media lodging is one of the most common production problems in mass finishing.
It happens when ceramic, plastic, porcelain, or steel tumbling media becomes trapped inside:
Holes
Slots
Threads
Grooves
Blind cavities
Cross holes
Internal channels
Undercuts
Recesses
Complex die cast structures
For simple parts, media selection is relatively straightforward.
For complex parts, it becomes much more difficult because the media must do two contradictory things:
It must reach the areas that need finishing.
But it must not become trapped inside the part.
This means media selection is not only a question of cutting ability.
It is also a geometry-management problem.
A finishing process can produce excellent burr removal and still be unsuitable for mass production if operators must manually remove lodged media from every part.
The goal should therefore be:
Achieve the required finishing result with the lowest practical lodging risk.
This guide explains how to prevent media lodging before production starts and how to design the machine, media, process, separation, and inspection system around complex part geometry.
Quick Summary
| Prevention Strategy | Why It Helps |
|---|---|
| Review part geometry before media selection | Identifies high-risk openings |
| Use the largest practical media | Reduces entry into small features |
| Avoid media dimensions close to openings | Reduces wedging |
| Consider media shape, not only size | Prevents rotational locking |
| Check worn media size | Prevents future lodging |
| Keep media out of unnecessary features | Simplifies production |
| Screen undersized media | Controls long-term risk |
| Validate separation | Reduces manual handling |
| Inspect threads and cavities | Prevents hidden media |
| Test real parts | Reveals geometry interactions CAD cannot fully predict |
The key principle is:
Do not choose media only for access. Choose media for access + free movement + reliable removal.
Why Complex Parts Have Higher Lodging Risk
Complex parts contain multiple features with different dimensions.
A single component may have:
Large external edges.
Small through holes.
Blind threaded holes.
Slots.
Grooves.
Internal pockets.
Cross-drilled channels.
Recessed ribs.
The media that is ideal for one feature may be dangerous for another.
| Part Feature | Finishing Need | Lodging Risk |
|---|---|---|
| External edge | Strong media contact | Low |
| Through hole | Edge finishing | Medium |
| Blind hole | Internal finishing | High |
| Thread | Burr removal | Very high |
| Slot | Edge smoothing | High |
| Cross hole | Internal burr removal | Very high |
| Deep cavity | Surface access | High |
| Internal channel | Cleaning/deburring | Very high |
This is why complex-part finishing should begin with geometry analysis.
Step 1: Review the Part Drawing First
Before choosing media, review the technical drawing.
Identify:
Minimum hole diameter
Maximum hole diameter
Blind-hole depth
Thread dimensions
Slot width
Slot depth
Groove width
Cross-hole intersections
Internal cavity openings
Narrow necks
Undercuts
A good media recommendation should compare these dimensions with the complete media geometry.
Create a Critical Opening List
For complex parts, make a simple table.
| Feature | Dimension | Needs Finishing? | Media Entry Allowed? |
|---|---|---|---|
| Hole A | — | Yes | Yes |
| Thread B | — | No | No |
| Slot C | — | Yes | Controlled |
| Blind Hole D | — | No | No |
| Cross Hole E | — | Yes | Test required |
This immediately makes media selection more logical.
Step 2: Decide Which Areas Actually Need Finishing
This is one of the most effective lodging-prevention strategies.
Not every hole needs media entry.
Suppose a CNC part has:
Sharp external edges.
Several internal threaded holes.
If the threads are already acceptable, there is no reason to allow media into them.
The better process may be:
Use larger media.
Deburr the external edges.
Keep media completely outside the threads.
This is often safer than using very small media simply to “reach everything.”
Finish Only What Needs Finishing
Ask:
Where is the burr?
Which surfaces are cosmetic?
Which holes need edge rounding?
Which threads must remain protected?
Which internal cavities are functional?
This can dramatically reduce lodging risk.
Step 3: Use the Largest Practical Media
A useful general rule is:
Use the largest media that can still reach the required finishing area.
Larger media usually provides:
Lower lodging risk
Easier separation
Better part cushioning
Fewer media pieces per batch
Less manual inspection
Smaller media provides:
Better access
Higher lodging risk
Harder separation
More pieces to manage
The best choice is not the smallest possible media.
Example
A part has:
20 mm external edges requiring deburring.
6 mm internal holes that do not need finishing.
Using 4 mm media may unnecessarily create lodging risk.
A larger media that cannot enter the 6 mm holes may be much safer.
Step 4: Avoid the “Almost Fits” Zone
The most dangerous media is often not:
Much larger than the opening.
Or much smaller.
It is the media that almost fits.
If media dimensions are close to the hole or slot size, it can enter and wedge.
| Media vs Opening | Risk |
|---|---|
| Clearly larger | Low entry risk |
| Much smaller and free-flowing | Can be acceptable after testing |
| Close to opening size | High risk |
| Same nominal size | Very high risk |
| Tapered media close to opening | Extremely high risk |
Avoid borderline geometry whenever practical.
Step 5: Consider Media Shape
Size alone is not enough.
A cone, cylinder, triangle, ball, and pin with similar dimensions can behave very differently.
| Media Shape | Main Lodging Concern |
|---|---|
| Cone | Wedges in round/tapered holes |
| Cylinder | Rotates inside slots |
| Angle-cut cylinder | Locks in grooves/slots |
| Ball | Lodges in round holes |
| Pin | Enters small holes and threads |
| Triangle | Can lodge in irregular openings |
| Pyramid | Can lock in tapered spaces |
| Ballcone | Wedges in holes |
| Special shape | Must be tested against actual geometry |
Always evaluate orientation.
Step 6: Check the Media’s Maximum Dimension
Do not look only at one nominal size.
For example, a triangular media may have:
Width.
Thickness.
Length.
Diagonal dimension.
One orientation may fit through an opening even when another does not.
For cylindrical media, check:
Diameter.
Length.
Diagonal rotation.
For cones, check:
Small end.
Large end.
Length.
Taper angle.
Step 7: Prevent Cone Wedging
Cone media is widely used because it is versatile.
However, it can wedge easily in round holes.
A cone can enter narrow end first and become stuck where its diameter matches the hole.
Possible prevention:
Use a larger cone.
Use a much smaller freely moving cone.
Use a non-tapered shape.
Prevent entry if internal finishing is not required.
Test actual hole tolerances.
Step 8: Prevent Cylinder Locking in Slots
Cylinders may enter slots lengthwise.
Once inside, they can rotate and become wider than the slot opening.
To prevent this:
Measure slot width.
Measure media diameter/thickness.
Measure media length.
Consider diagonal rotation.
Test whether the media can turn inside the slot.
Do not assume a media is safe simply because its width is smaller than the slot.
Step 9: Treat Threads as High-Risk Features
Internal threads are one of the most difficult geometries in mass finishing.
Media can lodge:
Between thread flanks.
At the bottom of blind threads.
Across thread entries.
Pins and small media are particularly risky.
If internal thread finishing is not required:
Keep media out.
If internal burr removal is required:
Test carefully.
Consider alternative deburring methods if complete media removal cannot be guaranteed.
Thread Protection Strategies
Possible approaches include:
Use larger media.
Mask or plug critical threads where practical.
Use another deburring operation.
Use media that cannot enter.
Inspect threads after finishing.
For high-volume production, manual media picking from threads should be avoided.
Step 10: Treat Blind Holes Differently from Through Holes
A through hole gives media two possible directions of movement.
A blind hole has only one exit.
This makes lodging much more likely.
Media can:
Drop to the bottom.
Rotate.
Pack together.
Become difficult to see.
For blind holes, the safest strategy is often:
Prevent media entry unless internal finishing is genuinely required.
Step 11: Review Cross Holes Carefully
Cross holes create complex internal intersections.
A media may:
Enter through one hole.
Move into the intersection.
Rotate.
Lock across another hole.
This can happen even when the media moves freely inside each individual bore.
Cross-hole parts should always be physically tested.
Step 12: Review Internal Cavities and Undercuts
Complex castings often include:
Deep pockets
Ribs
Internal chambers
Narrow entrances
Undercuts
Media can enter a large cavity but fail to exit because the opening is smaller or differently oriented.
Typical applications include:
Aluminum die cast housings
Valve bodies
Automotive castings
Pump components
Lock bodies
Complex zinc die castings
Ask:
Can media enter?
Can it rotate?
Can it fall behind a rib?
Can it exit automatically?
Step 13: Use Special-Shaped Media Only When It Solves a Real Geometry Problem
Special plastic shapes can help reach:
Deep recesses.
Slots.
Complex pockets.
The uploaded product report specifically notes special nipple-shaped plastic media for deep holes, slots, and recesses. The value of these shapes is geometry-specific; they still need to be matched to the actual opening dimensions and tested for reliable removal.
Special media should not be selected just because the part is “complex.”
It should solve a defined access problem.
Step 14: Consider Media Material
Media material also changes lodging behavior.
Ceramic Media
Advantages:
Strong cutting
Effective on steel and stainless steel
Lodging concerns:
Dense.
Can wedge firmly.
Can break when forced out.
Fragments may remain.
Plastic Media
Advantages:
Lighter.
Gentler.
Often suitable for aluminum, brass, zinc, and soft metals.
Lodging concerns:
Still wedges if geometry is wrong.
Can become difficult to remove from deep cavities.
Porcelain Media
Advantages:
Fine polishing.
Suitable for precision parts.
Lodging concerns:
Often available in very small sizes.
Pins and small shapes can enter tiny holes.
Steel Media
Advantages:
Long life.
Strong burnishing.
Lodging concerns:
High density.
Balls and pins can become tightly trapped.
Hidden steel media can cause downstream problems.
Step 15: Consider Media Wear Before Approving the Process
A process should not be approved based only on new media.
Ceramic and plastic media wear continuously.
Over time:
Media becomes smaller.
Edges become rounded.
Broken pieces appear.
Previously safe media may enter holes.
This is one of the main reasons lodging starts after months of stable production.
Design for Worn Media
Ask:
What is the new media size?
What will the media size be after significant wear?
At what size does it become dangerous?
What is the minimum allowed size?
Once this is known, the factory can screen out undersized media before lodging begins.
Step 16: Set a Minimum Media Size
A stable process should define:
Minimum usable media dimension
When media falls below that value:
Remove it.
Do not keep it in the bowl simply because it still has abrasive life.
The cost of discarded media may be much lower than the labor and risk created by lodging.
Step 17: Screen Media Regularly
Screening removes:
Undersized media
Broken media
Irregular fragments
Possible screening frequency depends on:
Media wear rate.
Daily production.
Critical opening dimensions.
Lodging sensitivity.
A high-risk precision part may need stricter screening than a simple steel bracket.
Step 18: Do Not Only Add New Media
Media top-up is necessary because ceramic and plastic media wear.
But adding new media without removing old undersized media creates:
Large size variation.
New media.
Medium media.
Tiny worn media.
This can actually increase lodging risk.
A better maintenance process is:
Screen → remove undersized media → add new media.
Step 19: Review Part Tolerances
The drawing may show one nominal hole size.
Production parts may vary.
If media is near the dangerous size:
A slightly larger hole may allow entry.
A slightly smaller hole may lock the media more tightly.
Include maximum and minimum part dimensions when evaluating lodging.
Step 20: Consider Burrs Themselves
A burr can change the effective opening size.
For example:
Media enters a slot.
The burr acts like a one-way edge.
Media moves past it.
Then cannot exit easily.
After deburring, later parts may behave differently.
This is another reason real-part testing matters.
Step 21: Test New and Worn Media Conditions
When possible, test:
New media.
Partially worn media.
Or simulate the expected lower media-size range.
The goal is to confirm that the process remains safe throughout media life.
Step 22: Keep High-Risk Features Out of the Media Path
Sometimes the part orientation or process can be redesigned so media has less opportunity to enter critical features.
This may be easier in:
Fixtures.
Compartmentalized systems.
Certain barrel processes.
Large parts.
However, standard vibratory finishing involves random movement, so orientation cannot always be controlled.
Step 23: Consider Fixture Finishing for Special Parts
For high-value or delicate parts, fixtures may help:
Prevent part-on-part damage.
Control orientation.
Protect specific surfaces.
Reduce media entry into certain features.
This is more complex and less common for general bulk finishing but can be useful for demanding applications.
Step 24: Separate Deburring Tasks
A common mistake is trying to make one media finish:
External edges.
Internal holes.
Threads.
Deep cavities.
Cosmetic surfaces.
all in one process.
Sometimes the better route is:
Pre-deburr difficult internal features.
Then mass finish external surfaces.
This can greatly simplify media selection.
Example
Part has:
Heavy cross-hole burr.
Cosmetic outer surface.
Instead of using very small aggressive media that lodges everywhere:
Remove the cross-hole burr separately.
Then use larger gentle media for the external finish.
This may reduce total process cost.
Step 25: Consider Alternative Deburring Methods for Inaccessible Features
Some internal burrs are simply poor candidates for standard mass finishing.
Possible alternatives may include:
Manual deburring
Brush deburring
Thermal deburring where appropriate
Electrochemical deburring where appropriate
Abrasive flow processes
Machining optimization
Specialized internal deburring
Mass finishing can then handle the remaining external surfaces.
The goal is not to force one process to do everything.
Step 26: Evaluate Machine Type
Different machines move media differently.
Vibratory Bowl
Good for:
General parts.
Bulk finishing.
Integrated separation.
But random circulation means media may enter holes from many orientations.
Centrifugal Disc
High energy.
Suitable for small robust parts.
More aggressive movement may increase both finishing access and lodging forces.
Centrifugal Barrel
Suitable for precision parts.
Uses fine media effectively.
Small-media lodging must be controlled carefully.
Rotary Barrel
Gentler movement.
Longer processing.
Can still create media lodging.
Magnetic Polishing
Uses small steel pins.
Excellent access to some fine details.
But pin lodging in holes and slots is a critical consideration.
Machine choice does not eliminate geometry risk.
Step 27: Design Separation Together with Media Selection
A production-ready process must answer two questions:
Can the media finish the part?
Can the media be separated efficiently?
Possible separation systems include:
Integrated vibratory screen.
Standalone vibratory separator.
Magnetic separator for suitable media.
Manual separation for low-volume special parts.
The uploaded product report also treats vibratory separators and magnetic separation as part of the complete machine + media + auxiliary equipment solution, rather than an afterthought.
Free Media vs Lodged Media
Automatic separation handles free media.
It does not solve wedged media.
This distinction is critical.
A separator may show 99% separation efficiency but still leave one ceramic cone trapped inside every tenth part.
That is still a production problem.
Step 28: Build Inspection into the Process
For complex parts, post-finishing inspection may include:
Visual inspection.
Air blowing.
Hole probing.
Thread inspection.
Weight checking in special applications.
Functional assembly.
Borescope inspection for critical internal features.
Inspection effort should match the risk.
Hidden Media Is the Highest-Risk Problem
Visible lodged media is inconvenient.
Hidden lodged media is more dangerous.
It can cause:
Blocked fluid channels.
Assembly failure.
Customer complaints.
Contamination.
Medical-device risk in critical applications.
Downstream processing problems.
For critical parts, media-removal validation should be part of process approval.
Step 29: Use Air Blowing as Secondary Control
Air blowing can remove loose media from:
Open holes.
Slots.
Threads.
Recesses.
But it should be a backup control—not the primary fix for poor media selection.
If every part requires aggressive manual air blowing, review the process.
Step 30: Use Water Flushing Where Appropriate
Water flushing can help clear loose media from:
Channels.
Open cavities.
Through holes.
It is less effective for tightly wedged pieces.
For steel parts, remember that additional water exposure also affects drying and corrosion protection.
Step 31: Check Lodging After Drying Too
Media can sometimes remain hidden in wet parts and become easier to see after:
Drying.
Air blowing.
Handling.
Always inspect the final part, not only the part immediately after separation.
Step 32: Quantify Lodging Frequency
Do not describe the problem only as:
“Sometimes media gets stuck.”
Measure it.
Example:
1 lodged media per 20 parts.
3 lodged pieces per 100 parts.
15% of parts require manual removal.
This helps calculate the real cost.
Lodging Cost Example
Suppose:
5,000 parts/day.
10% require manual media removal.
Removal takes 15 seconds each.
That creates:
500 parts × 15 seconds = 7,500 seconds
More than 2 hours of labor every day.
A slightly more expensive media with lower lodging may easily be cheaper overall.
Step 33: Evaluate Lodging Risk Alongside Cycle Time
Media A:
20-minute cycle.
10% lodging.
Media B:
25-minute cycle.
No lodging.
Media A appears faster.
But if manual removal and inspection take significant labor, Media B may provide a lower total production cost.
Step 34: Create a Media Lodging Risk Map
For complex parts, mark features as:
Low risk.
Medium risk.
High risk.
| Feature | Risk | Control |
|---|---|---|
| Large open edge | Low | Normal finishing |
| Large through hole | Low/medium | Check media size |
| Narrow slot | High | Shape/rotation test |
| Blind threaded hole | Very high | Prevent entry |
| Cross hole | Very high | Sample test |
| Deep cavity | High | Exit test |
This helps guide media selection.
Step 35: Approve the Complete Process, Not Only Surface Finish
A sample should not be approved just because:
Burr removed.
Surface looks good.
Approval should also include:
No unacceptable lodging.
Acceptable separation time.
No hidden media.
No thread damage.
Repeatable removal.
Acceptable labor.
A production process must work operationally.
Example 1: CNC Aluminum Housing
Features:
External machining burrs.
Deep pockets.
Several threaded holes.
Goal:
Smooth external edges before anodizing.
Best strategy:
Use plastic media large enough to remain outside the threaded holes where possible.
Select shape for external edges and pockets.
Avoid unnecessary thread entry.
Check anodized result.
Example 2: Stainless Steel Valve Body
Features:
External burrs.
Cross holes.
Internal channels.
Goal:
General deburring.
Risk:
Ceramic media can enter and lodge in cross-hole intersections.
Possible strategy:
Use larger ceramic media for external surfaces.
Use another method for internal cross-hole burrs if necessary.
This may be safer than forcing small ceramic media through the channels.
Example 3: Zinc Die Casting
Features:
Complex recesses.
Light flash.
Decorative surface.
Goal:
Gentle smoothing before plating.
Possible strategy:
Use plastic media.
Test special geometry only where recess access is required.
Avoid media sizes close to cavity entrances.
Check plating after testing.
Example 4: Stainless Steel Nut
Features:
Internal thread.
External sharp edges.
Goal:
External deburring and brightening.
Possible strategy:
Keep abrasive media out of the internal thread.
Use larger media for external deburring.
Add steel burnishing later if brightness is required.
Example 5: Medical Precision Part
Features:
Small holes.
Channels.
Tight tolerances.
Goal:
Fine deburring and surface smoothing.
Process priorities:
Complete media removal.
Dimensional stability.
Controlled surface roughness.
Low contamination.
The safest media process may not be the fastest process.
Example 6: Laser Cut Bracket
Features:
External perimeter.
Multiple narrow slots.
Goal:
Edge rounding.
Possible strategy:
Select media that strongly contacts external edges but cannot wedge in slots.
If internal slot edges also need finishing, test a second media size or alternative process.
Lodging Troubleshooting Table
| Situation | Prevention Direction |
|---|---|
| Cone stuck in hole | Change size or shape |
| Cylinder stuck in slot | Check rotation and diagonal size |
| Pins stuck in threads | Keep pins out or use alternative process |
| Lodging begins after months | Screen worn media |
| Only some parts lodge | Check part tolerances |
| Broken media lodged | Screen fragments |
| Media trapped in cavity | Review exit geometry |
| Automatic separator misses media | Media is physically lodged |
| High manual removal | Redesign media selection |
| Hidden media risk | Add inspection/alternative process |
Process Development Workflow
A practical lodging-prevention workflow is:
- Review the drawing.
- Identify all openings.
- Mark which features need finishing.
- Mark which features should exclude media.
- Select candidate media material.
- Select candidate shape.
- Compare every media dimension with every critical opening.
- Consider possible orientations.
- Consider worn media size.
- Run a real-part test.
- Check finishing result.
- Inspect every high-risk feature.
- Count lodged media.
- Test separation.
- Test air/water removal if needed.
- Compare alternative media.
- Define minimum acceptable media size.
- Define screening frequency.
- Record the process.
Buyer Checklist for Complex Parts
| Checkpoint | Confirmed |
|---|---|
| Technical drawing reviewed | Yes / No |
| All holes listed | Yes / No |
| Blind holes identified | Yes / No |
| Threads identified | Yes / No |
| Slots measured | Yes / No |
| Cross holes identified | Yes / No |
| Cavities reviewed | Yes / No |
| Burr locations marked | Yes / No |
| Features needing no finishing marked | Yes / No |
| Media material selected | Yes / No |
| Media shape reviewed | Yes / No |
| All media dimensions reviewed | Yes / No |
| Worn-media condition considered | Yes / No |
| Lodging test completed | Yes / No |
| Separation test completed | Yes / No |
| Minimum media size defined | Yes / No |
| Screening plan defined | Yes / No |
| Final inspection defined | Yes / No |
What Information Should You Send to the Supplier?
For complex-part media selection, send:
| Information | Why It Matters |
|---|---|
| Part photos | Shows overall geometry |
| Technical drawing | Essential for opening analysis |
| Material/alloy | Determines media type |
| Part size and weight | Helps select machine/media |
| Burr location | Defines where media must reach |
| Hole diameters | Determines entry risk |
| Blind-hole depth | Determines exit risk |
| Thread sizes | Identifies high-risk features |
| Slot width/depth | Helps check rotation |
| Cross-hole dimensions | Identifies locking risk |
| Cavity openings | Helps evaluate entry/exit |
| Critical surfaces | Helps avoid damage |
| Target finish | Determines cutting strength |
| Current media | Helps diagnose lodging |
| Current lodged-media photos | Shows locking mechanism |
| Batch quantity | Determines separation practicality |
| Daily output | Determines labor impact |
For complex parts, a technical drawing is often far more useful than a general product photo alone.
Sample Testing Process
A useful real-part lodging test should include:
- Inspect the raw parts.
- Confirm every critical opening.
- Select candidate media.
- Measure actual media dimensions.
- Record new-media size.
- Run the finishing cycle.
- Check burr removal.
- Perform normal separation.
- Inspect through holes.
- Inspect blind holes.
- Inspect threads.
- Inspect slots.
- Inspect cross holes.
- Inspect cavities.
- Count lodged pieces.
- Remove loose media with the planned production method.
- Check whether manual picking remains necessary.
- Rinse and dry.
- Inspect again.
- Compare another media option if needed.
What Should the Process Report Include?
| Report Item | Purpose |
|---|---|
| Part geometry summary | Identifies risk |
| Critical opening dimensions | Defines media limitations |
| Machine | Defines movement |
| Media material | Defines finishing type |
| Media shape | Defines contact/locking behavior |
| New media size | Initial condition |
| Minimum media size | Long-term control |
| Processing time | Production parameter |
| Burr result | Confirms finishing |
| Lodging count | Quantifies risk |
| Separation method | Confirms production handling |
| Additional removal method | Defines labor |
| Final inspection | Confirms hidden-media control |
| Recommended process | Production recipe |
Practical Recommendations
Review the drawing before choosing media.
Identify which internal features genuinely need finishing.
Keep media out of threads, blind holes, and cavities when internal finishing is unnecessary.
Use the largest practical media that still reaches required burrs.
Avoid media dimensions close to opening dimensions.
Evaluate full media geometry, not only nominal size.
For cones, check wedging.
For cylinders and pins, check rotation.
Consider media wear from the beginning.
Set a minimum safe media size.
Screen out undersized and broken media.
Do not rely on automatic separation to remove physically lodged media.
Use air blowing or flushing only as secondary controls.
Test the complete process with real parts.
Include lodging rate and removal labor when comparing media options.
Common Mistakes to Avoid
Do not select the smallest media just because the part is complex.
Do not assume every cavity needs media entry.
Do not ignore media orientation.
Do not compare only media diameter.
Do not approve a process using only new media.
Do not forget that media gets smaller during production.
Do not keep worn media forever.
Do not assume separators solve lodging.
Do not accept high manual media-removal labor as normal.
Do not optimize cycle time while ignoring separation and inspection.
Do not approve a process without checking hidden holes and threads.
Conclusion
Preventing media lodging in complex parts requires more than choosing a different tumbling media size.
A reliable process begins by understanding the complete part geometry and deciding exactly where the media must—and must not—go.
The key factors are:
part geometry + media material + media shape + media size + media orientation + worn media size + separation + inspection
For many complex parts, the safest process uses the largest practical media that can still reach the required finishing areas while staying outside critical holes, threads, and cavities.
When internal finishing is required, the media must be able to enter, move, and exit freely—not simply fit through the opening.
Long-term production also requires control of media wear. A process that is safe with new media may begin lodging after the media becomes smaller, which is why screening and minimum media-size limits should be included in the production recipe.
ShinyStar Machinery develops mass finishing processes based on real part geometry rather than recommending media only from overall part size.
If you are processing complex CNC parts, die castings, valve bodies, threaded components, medical parts, or parts with holes, slots, cross holes, and cavities, send us your part photos, technical drawings, material, burr locations, opening dimensions, current media, target finish, batch quantity, and daily output.
Our team can test different machine + media + compound combinations, evaluate lodging and separation, and recommend a production process designed for both finishing quality and reliable media removal.